Teisinis statusas
Patentas neįsigaliojo (pagal EPK)
| (51) | INT.CL. | C22C 38/00 | |
| C22C 38/18 | |||
| C22C 38/54 | |||
| C21D 8/02 | |||
| C21D 6/00 | |||
| C22C 38/02 | |||
| C22C 38/04 | |||
| C22C 38/06 | |||
| C22C 38/26 | |||
| C22C 38/28 | |||
| C22C 38/32 | |||
| B32B 15/01 |
| (11) | Patento numeris | 2687617 |
| (13) | Dokumento rūšis | T |
| (96) | Europos patento paraiškos numeris | 12756952.3 |
| Europos patento paraiškos padavimo data | 2012-03-05 | |
| (97) | Europos patento paraiškos paskelbimo data | 2014-01-22 |
| (45) | Paskelbimo apie Europos patento išdavimą data | 2020-05-20 |
| (46) | Apibrėžties vertimo paskelbimo data |
| (86) | Numeris | PCT/JP2012/055583 |
| Data | 2012-03-05 |
| (87) | Numeris | WO 2012/124528 |
| Data | 2012-09-20 |
| (30) | Numeris | Data | Šalis |
| 2011055947 | 2011-03-14 | JP |
| (72) |
HATANO, Masaharu, JP
MATSUYAMA, Hiroyuki, JP
YAMAGISHI, Akihito, JP
HANSAKI, Naoto, JP
ISHIMARU, Eiichiro, JP
|
| (73) |
Nippon Steel & Sumikin Stainless Steel Corporation,
6-1, Otemachi 2-chome, Chiyoda-ku Tokyo 100-0004,
JP
|
| (54) | HIGH-PURITY FERRITIC STAINLESS STEEL SHEET WITH EXCELLENT CORROSION RESISTANCE AND ANTI-GLARE PROPERTIES |
| HIGH-PURITY FERRITIC STAINLESS STEEL SHEET WITH EXCELLENT CORROSION RESISTANCE AND ANTI-GLARE PROPERTIES |